  • × where they were held for 1 h and then cooled to room temperature. The microhardness of the as-electrodeposited and as-annealed samples was measured with a Shimadzu model HMV-2 Micro Hardness Tester operating with an applied load of 10 g (98.07 mN)
 全选  【符合条件的数据共:1条】

来源:Journal of the Brazilian Chemical Society , 2006

作者:Lima-Neto, Pedro de, Silva, Gecílio P. da, Correia, Adriana N.

关键词:corrosion;crystallization behavior;...